HFRR Tester Overview
Main Features:
- Real-time down force control
- Oscillation frequency from 1 to 200 Hz
- Oscillation amplitude from 10 µm to 2.8 mm
- Friction force measurements with piezo load sensors
- Temperature: Room to 150 °C (cooling and up to 400°C options available)
- Load range up to 20 N (other load ranges available)
Evaluate lubricity, predict additive performance, and study friction and wear with our HFRR high-frequency reciprocating rig.
This next-generation Rtec Instruments HFRR testing machine features programmable force control (no dead weights), combined with piezo sensors to measure real-time friction. Its ease of use and flexure-based design make the tester highly reliable and repeatable.
Samples can be tested either from the field or for research purposes. The FFT-M provides a fully automated, computer-controlled test. Setup is easy, with calibration supported by standard oils and samples.
Each tester conforms to several ASTM standards, including the widely used ASTM D6079. In addition to standard testing, the wide stroke, frequency, and load ranges allow the development of new custom test methods—making it ideal for evaluating next-generation fuel additives.
Need help or have a question?
ASTM Tests and More
Our lubricity tester, the FFT-M, performs friction and wear analysis on petroleum products.
ASTM D7688
Standard Test Method for Evaluating Lubricity of Diesel Fuels by the High-Frequency Reciprocating Rig (HFRR) by Visual Observation.
ASTM D6079
Standard test method for evaluating lubricity of diesel fuels by the high frequency reciprocating
ISO 12156-1
Diesel Fuel – Assessment of Lubricity Using the High Frequency Reciprocating Rig (HFRR). Part 1 Test Method.
CEC F-06-A-96
Measurement of Diesel Fuel Lubricity
JPI-5S-50-98
Gas Oil – Testing Method For Lubricity.
IP 450/2000
Diesel Fuel – Assessment of Lubricity Using the High Frequency Reciprocating Rig (HFRR).
Choose Your Model
Rtec offers two solution for your fuel lubricity evaluation. Run HFRR test on our Multi Function Tribometer MFT-5000 platform or on dedicated single function HFRR tester covered on this page.

Single Function HFRR Tester
Bench top, small foot print HFRR instrument platform dedicated to HFRR tests only.
Multi Function Tribometer Model MFT-5000
In addition to HFRR testing, several other friction, tribology, and wear modules are available on the same MFT-5000 platform. SRV, block on ring, pin on disk, and more.
Typical Test Analysis
- Evaluate lubricity of diesel and aviation fuels
- 1mm 50 Hz, 200 g normal force
- 6 mm diameter ball, 10 mm diameter x 3 mm thick disc
- Humidity control and monitoring
- Temperature: 70°C
- Wear scar and friction analyses
Need Versatile HFRR Testing?
Need SRV Testing?
Want to learn more?
Get in touch, and request a demo.
recommended
Information
© Copyright 2021 Rtec-Instruments - All Rights Reserved