3D Scratch Testing With The MFT Series Overview
Main Features:
- 3D Profiler and scratch data automatic correlation
- Nano scratch, micro scratch, macro scratch on same tester
- High repeatability because of rigid design
- Automatic reports
The 3D Scratch Test module quantifies coating substrate systems. It measures scratch adhesion, scratch hardness, and marr resistance at nano, micro and macro scale. In-line integrated 3D profilometer allows to analyze failures with high resolution. The profilometer correlates effect of roughness, features, and more, on the measured properties. Advanced patented capacitive sensors measure force and penetration depth with resolution needed to differentiate coatings at any scale.
Need help or have a question?
Learn More About The Platforms
The MFT Series Tribometers
Explore our MFT Series Tribometers for versatile surface and material testing.
Coatings Adhesion, Scratch, and Mar Resistance
The scratch test quantifies the adhesion and scratch hardness of coatings. Thinner coatings are finding their way into every aspect of our life with new deposition methods and technologies. Coatings are applied to LCD displays, phones, cutting tools, gems, glass, automobiles, and medical devices. Quantitative coating adhesion scratch testing is a simple, practical test that the MFT tribometers provide for comprehensive coating scratch testing evaluation.
Friction, Wear, and Coating Failures Data Correlation
Pre Test Image
Sample moves under 3D profilometer to measure surface topography
Scratch test
Single or multiple scratches using predefined recipes are performed
Post Test Image
The sample moves under the profilometer to analyze scratch area
Report
Automatic image, adhesion, friction, depth, and roughness correlation reports are created.
3D Scratch Test nm to mm, Thick Coatings, and High Temperature
A scratch test requires applying a load on the sample that needs testing with a spherical or custom tip. During load application, the sample moves at a constant velocity and several parameters such as Friction (Fx), Down force (Fz), Coefficient of friction (COF), displacement (Z), acoustic emission (AE), and temperature are measured in situ.
Sensors and Chambers
Application specific solutions
Environmental chambers and a variety of sensors create numerous test variations that replicate real-life scenarios.
Sensors
Various sensors on coating scratch adhesion tester allows gathering of more information during the test.
Electrical Contact Resistance
Measure point of coating failure by looking at resistance change during the scratch.
Acoustic Emission
Measures sound signal during the scratch, that may point to onset of coating failures.
Potentiostat
Provides scratch corrosion studies.
Environmental Chambers
Temperature, Humidity, and More.

Scratch Setup With In-line Profiler

Scratch With Rockwell Tip

Scratch With Cutting Tool
The Scratch Test Solution
Due to multiple configurations, the MFT Series is used extensively across a wide range of industries:
Aerospace
- Thermal Spray Coatings
Automotive
- Marr Resistance, Scratch Adhesion
- Thermal Spray Coatings
Bio-materials
- Scratch Resistance
Ceramics
- Scratch Resistance
Hard Coating
- Scratch Resistance
Metal
- Scratch Hardness
- Scratch Resistance
Optics and Glasses
- Scratch Resistance
Pharmaceutical
- Scratch Resistance
Polymer
- Scratch Resistance
Semicon
- Scratch Resistance
Need Focused Indentation and 3D Scratch Testing?
Take a look at Rtec-Intstruments’ Indentation and Scratch Tester, the SMT-5000.
Want to learn more?
Get in touch, and request a demo.
recommended
Information
© Copyright 2021 Rtec-Instruments - All Rights Reserved