Home > Tribometers > Applications >
ASTM D6078-04
Lubricity of Diesel Fuels by the Scaffing Load Ball-on-Cylinder Lubricity Evaluator
SLBOCLE
Evaluate the lubricity (load carrying ability) of diesel fuels using a scuffing load ball-on-cylinder lubricity evaluator (SLBOCLE).
Summary of the ASTM D6078-04 Standard Method
This test method evaluates the lubricity (load carrying ability) of diesel fuels using a multi-functional tribometer MFT 5000.
In this test method the lubricity of a fluid is evaluated by the minimum applied load in grams that, at any time during the test, will produce a friction coefficient greater than 0.175 between a stationary ball and a fluid-wetted rotating ring operating under defined conditions.
Applications
This test method is applicable to middle distillate fuels, such as Grades Low Sulfur No. 1 D, Low Sulfur No. 2 D, No. 1 D, and No. 2 D diesel fuels, in accordance with specification D975; and other similar petroleum-based fuels which can be used in diesel engines.
It is not known that this test method will predict the performance of all additive/fuel combinations.
Lubricity of Diesel Fuels Test Parameters
| Balls: | Chrome alloy steel, made from AISI standard steel No. E-52100, with a diameter of 12.7 mm, Grade 5 to 10. EP finish Carburized steel, having a Rockwell Hardness C Scale Number of 58 to 62 |
| Ring: | SAE 8720 steel, having HRC number of 58 to 62 |
| Force: | linear increasing (range 500 g to 5000 g) |
| Test Duration: | Until COF crosses 0.175 |
| Speed: | 525 rpm |
| Temperature: | Ambient -25 °C |
| Humidity: | 50% |
| Lubrication: | Lubricating Liquid |
| Data: | Normal Force (Fz) Friction (Fx) Coefficient of Friction Humidity (RH) |
Lubricity of Diesel Fuel Data Summary
ASTM D6078-04 test results are reported below. The load at which the COF crosses 0.175 is reported along with the wear scar diameter in the final report.
More on the Multi Function Tribometer (MFT-5000) Hardware
- Load sensor (100 N)
- Block on ring drive
- Humidifier
- Temperature chamber
- Block holder
- Liquid container for block on ring drive