Tribocorrosion Module Information
- Integrated 3 Electrode Potentiostat
- Up to 70°C temperature (optional 150°C)
- Upper or lower conductive samples
Why Tribocorrosion? Wear and corrosion involves several mechanical and chemical processes. The combination of these processes results in significant interaction that may occur beyond the individual contributions of mechanical wear and corrosion. Tribocorrosion studies help quantification of this wear corrosion synergism, or interaction, to minimize overall material loss and understand systems better.
Rtec Tribocorrosion tester cell mounts on the MFT series (Tribometer) or the SMT-5000 (Indentation and Scratch Tester). It equips a robust 3 electrode measurement system. During the test, the cell simultaneously measures real-time current, voltage, friction, wear, temperature, down force, and acoustic emissions.
Brauchen Sie Hilfe oder haben Sie eine Frage?
Learn More About The Platforms
The MFT Series Tribometers
Explore our MFT Series Tribometers for versatile surface and material testing.
Features
Rtec Tribocorrosion tribometer contains various features to improve testing capabilities.
Electrochemical Cell + Tribometer Combination
Tribocorrosion Test Modes
- Tribology
- Scratch Adhesion
- Hardness
- Fretting
Test Samples
Analysis
Setup
To investigate synergy of wear and corrosion of steel, the tests were carried out under cathodic and no cathodic protection conditions. We conducted 3 different load conditions (10, 100, 200 N at 2 Hz sliding frequency) at 70°C. The electrochemical polarization tribocorrosion tests were performed with a standard Ag/AgCl reference electrode and a platinum counter electrode.
OCP – Oper Circuit Potential (Ecorr)
The plot below shows the open circuit corrosion potential, Ecorr obtained from the integrated potentiostat.
Results
The figure below shows the wear rate difference between the cathodic and non cathodic polarization conditions. The difference of the wear rate shows the synergy of the chemistry used during the test.
Conclusion
This corrosion tribology testing showed the importance of tribocorrosion studies. The wear loss rate attributed between mechanical vs mechanical + corrosion test was significantly different.
Solution To
-
Bio-materials
-
Coatings
-
Lubricants
-
Metals
-
Metal Working Industry
Need More Versatility?
Need Compact Tribology?
Learn about our benchtop Multi Function Tribometer, the MFT-2000.
Möchten Sie mehr erfahren?
Kontaktieren Sie uns und fordern Sie eine Demonstration an.
recommended
Information
© Copyright 2021 Rtec-Instruments - All Rights Reserved