Wear Test Parameters :

Balls:Steel Balls material AISI standard steel E52100 Grade 25 EP (100Cr6)
Ball diameter:12.7 mm
Normal Force:392 N
Test Duration:60 minutes
Speed:1200 rpm
Temperature:75 °C
Lubrication:Test Grease
Data:Torque (Tx)
Normal Force (Fz)
Rotation Speed (rpm)
Temperature (°C)
Acoustic Emission AE

Data Summary

 The quantitative information measured on Rtec-Instruments MFT-5000 Four Ball set up provides insights into the lubrication and wear resistance performance of the greases. 

The average wear scar diameter of the three lower balls is reported in the final report. 