Overview
Main Features:
- Up to 200 PSI pressure
- Real-time down force control
- In-line friction and wear
- Patented capacitive high pressure force sensor
- -35 to 100°C Temperature Range
- Load Range 5 N to 2000 N
Study friction and wear of various materials for valves, seals, liners, bearings, compressors, and much more. Tester supports controlled test environments at high pressure. The tribological behavior of high pressure application products depends heavily on gas environment and pressure. Chemical reactions and dissolution rates play an important role in the processes at contacting surfaces.
Rtec Instruments high pressure tribometer runs ball on disk and pin on disk tribology test under high pressure. Rigid chamber construction, wide load range up to 2000 N to simulate several high pressure tribology applications.
Need help or have a question?
High Pressure Tribometer Features
Real-time programmable force control, patented capacitive sensors to measure friction, in-line total wear scar depth, and temperature. The ease of use and safe operations makes this tester highly reliable and repeatable.

Temperature Control
Integrated chillers and heaters control test temperature from -35 to 100 °C during the test.

Force Sensors
The patented force sensor has no effect on force measurement due to high pressure or gases in the chamber.
Safety
Each chamber is ASME certified and stamped for pressure rating.
The High Pressure Tribometer Solution
The high pressure tribometer is used across a wide range of industries that use high pressure environments
-
Compressor
-
Referigerant
-
Aerospace
-
Seals
-
Lubricants
-
High Pressure Coatings
-
Linear and Rings
-
Turbines
The MFT-5000 Has More To Offer
Want to learn more?
Get in touch, and request a demo.