Summary of the ASTM G176-03 Standard Method

This test method covers laboratory procedures for determining the resistance of plastics to sliding wear. The test utilizes a block-on-ring friction and wear testing machine to rank plastics according to their sliding wear characteristics against metals or other solids.

A test block is loaded against a test ring that rotates at a given speed for a given number of revolutions. Block scar volume is calculated from the block scar width, and ring scar volume is calculated from ring weight loss.

The friction force required to keep the block in place is continuously measured during the test with a load cell. These data, combined with normal force data, are converted to coefficient of friction values and reported.

Sliding Wear Parameters

Ring:Outer diameter of 35 mm
Block:Width 6.35 mm
Force:44 N
Test Duration:20 hr
Speed:200 rpm
Temperature:Ambient 25 °C
Data:Normal Force (Fz)
Friction (Fx)
Coefficient of Friction
Temperature (°C)
Humidity (RH)

Data Summary

Test results are quickly reported. The real-time coefficiant of friction (COF), down force, and wear data are simulatiously recorded.


More on the Multi Function Tribometer (MFT-5000) Hardware

  • Load sensor (500 N)
  • Block on ring drive
  • Block holder
  • Liquid container for block on ring drive

Ready to take your tribology
research to the next level?

Discover Rtec Instruments' cutting-edge solutions and see how our technology can empower your work.

Contact our experts