Summary of the Standard

This note describes a commonly used standard for grease testing. This method is used to assess the load carrying properties of lubricating greases under
extreme pressure conditions.Rtec-Instruments Multi-function Tribometer (MFT-5000) with Four-Ball extreme pressure module can be used to evaluate wear and erosion resistance of test greases.

The test is performed by rotating a ball against three balls in a container packed with the test grease at various contact pressures till failure is observed. Three determinations are made and reported:

  • Load-Wear Index
  • Weld Point, by means of the Four-Ball Extreme Pressure (EP)
  • Last non-seizure load (LNSL).

Parameters

Balls:Steel Balls material AISI standard steel E52100 Grade 25 EP (100Cr6)
Ball diameter:12.7 mm
Normal Force:Step increasing load (6, 8, 10, 13,16, 20, 24, 32, 40, 50, 63, 80, 100, 126, 160, 200, 250, 315, 400, 500, 620, 800) Kgf*
Test Duration:10 seconds for each step
Speed:1770 rpm
Temperature:Ambient (23 °C)
Lubrication:Grease applied
Data:Torque (Tx)
Normal Force (Fz)
Rotation Speed (rpm)
Temperature (°C)
Acoustic Emission AE

ASTM D2596 Standard Set-up

These tests are done using Rtec-Instruments Multi Functional Tribometer MFT 5000. During the test in-line torque, down force, acoustic emission, electrical contact resistance and temperature values are recorded and reported.

The test involves increasing load in steps of 10 seconds each till the balls are welded representing abrasive wear. The linear loading mode of MFT-5000 tester also allows to run the same test in one step by applying a linearly increasing force at a controlled rate instead of multiple steps at constant load. This can be used as an efficient, high through put method of grease analysis.


Data Summary

Representative test results are reported below indicating failure at 620 Kg. The load at which the balls weld together, and the last non-seizure load is reported.

The load wear index is calculated by measuring the wear scar diameters on the lower three balls. Other tribological properties such as friction coefficient and acoustic emission can also be measured real time.


More on the Multi Function Tribometer (MFT-5000) Hardware

  • Quad force load sensor (10,000 N)
  • Torque sensor (22.6 Nm)
  • Upper rotary module
  • Four-ball module container assembly
  • Temperature chamber
  • Integrated 3D profilometer

Ready to take your tribology
research to the next level?

Discover Rtec Instruments' cutting-edge solutions and see how our technology can empower your work.

Contact our experts