Fretting Wear Tester Overview
- 10 µm to 2.8 mm Stroke
- 1 to 300 Hz frequency
- High frequency piezo Sensors
- Electromagnetic Coils
Brauchen Sie Hilfe oder haben Sie eine Frage?

A Fretting Machine Like No Other
Test the surface damage that occurs between two contacting surfaces. Analyze two-body abrasion, adhesion, and/or fretting fatigue wear.

Down Force Control
Real time down force control to account for contact wear.

Voice Coil
Electromagnetic actuator that imparts linear reciprocating motion. Dependent on the test additional coils can be installed on the tester to double the force range

High Accuracy Position Control
The most accurate and precise displacement control in the market. Up to 1nm resolution and micron level of accuracy. Extremely low noise. High responsiveness for dynamic performance of system.

Environmental Control
Study fretting wear across a wide range of temperature.

Unmatched Waveform Control
Without the friction of rolling or bearing, the magnetic flexure based design provides the control required for the most sensitive of tests. The unique controller adjusts to friction changes to maintain the stroke control in real-time.

Friction Measurement
The fretting tester comes with high frequency piezo sensors to measure real-time friction. Ultra low noise amplifiers aids in detection of minute changes in friction with ease.

Additional In-line Sensors
Sensors such as acoustic emission to detect onset of cracks, and ECR to measure surface resistance changes to gain more insight on the material interface.

Liquid Containers, Sample Holder
Customizable liquid and sample holders for standard and non standard tests.
Choose Your Fretting Tester Model
Difference in Voice Coil Power For Friction Force
All Rtec Fretting testers are constructed on flexure based designs. The motion is imparted using electromagnetic actuators with real time stroke and wave form correction controllers. The difference in model lies in the power the coil can impart during the test.

FFT-M Series
Up to 500 N Down Force (Bench Top, Single or Dual Medium Power Coil)

FFT-1
3000 N Down Force (Floor Standing, Single High Power Coil)

FFT-2
5000 N Down Force (Floor Standing, Dual High Power Coil)
Data and Analysis
FFT series fretting wear testing instruments are optimize for friction, wear, and fretting fatigue tests at small amplitude and high frequency.

Fretting Loops
Rigid design with accurate real-time friction force allows the measure of fretting loops at different temperatures, and loads.

Real Time Friction Curves at 300 Hz, 3000 N
The graph shows real-time friction data at 300 Hz, 2300 N test on dry material fretting test.

Fretting Failure Marks
Rtec 3D profilometer allows to create 3D images of surfaces with ease.
Fretting Wear Tester Solutions
Due to multiple fretting options, the fretting tester FFT Series is used extensively across a wide range of industries:
Aerospace
- Wear Resistance
- Fretting
- Thermal Spray Coatings
- High Temperature
Automotive
- Fretting and Wear Resistance
- Engine Related Tests
- Tribology, Friction, and Wear
Bio-materials
- Corrosion
- Fretting
Ceramics
- Wear Resistance
- Fretting and Friction Testing
Lubricants
- HFRR
- Wear Resistance and Friction
Metal
- Fretting
- Tribology and Friction Testing
Optics and Glasses
- Fretting and Wear Resistance
Pharmaceuticals
- Wear and Friction
Semicon
- Fretting
- Wear Resistance
- Tribology and Friction Testing
Need Versatile Fretting Testing?
Möchten Sie mehr erfahren?
Kontaktieren Sie uns und fordern Sie eine Demonstration an.
recommended
Information
© Copyright 2021 Rtec-Instruments - All Rights Reserved